Alligatoring
back to index • next page >
Description
Many wide patterned cracks in the paint film with the appearance of alligator scales.
Probable Cause
-
Usually multiple coats of naturally ages oil based paints that have become brittle and start cracking.
-
Topcoat’s inability to bond smoothly to a glossy undercoat.
-
Insufficient drying time between coats.
-
A hard coating over a soft primer.
Solutions
-
Remove all of the old paint by scraping and sanding.
-
A power washer is recommended for larger areas to shorted the removal time.
-
The best way to avoid future alligatoring is to properly prepare the surface and paint with a high quality primer/finish coat.